GLASS INVEST for pouring glass 1 kg
Ceramic material used for pouring glass objects.
Tax rate
22 %
Price with VAT:
5,86 €
ADVANTAGES
- smooth cast walls
- fast curing
- simple demolding
USAGE
- powder and water temperature 18-22°C
- water temperature over 30-35°C shortens the curing time, lower temperatures elongate it
- mixing ratio may variate within the prescribed ratio according to the shape's complexity
- pour the powder in the water, stir thoroughly, taking care not to mix in too much air (air bubbles may form
- vacuum the mixture if possible
- cure at room temperature for at least 120 minutes before heating
- evaporate the wax – heat for at least 3 hours
- fill the cuvette with glass granules and heat up to 900°C
- waiting time at 200°C is a few hours
- heating time at end temperature is 20-40 hours
- cooling time is approx. 4 days
- demold after cooling to room temperature